Aluminium tubes, prefabricated beams and other components are widely used throughout the scaffolding industry. Whilst aluminium is not as stiff as steel and will deflect more when subjected to equivalent loads, it is much lighter and provides great advantages with regard to manual handling or the reduction weight.
As aluminium couplers are not readily available, aluminium tube and beams are invariably connected with steel couplers and joint pins. Unfortunately, when two dissimilar metals such as aluminium and steel are in contact, a phenomenon known as ‘galvanic corrosion’ can occur where the corrosion of one of the metals, in this case aluminium, can be greatly accelerated. In severe cases this could seriously affect the integrity of the scaffold structure.
This guidance gives details of various methods available for satisfactorily securing scaffold boards to prevent movement. Users should satisfy themselves when/which boards require tying down and that any proprietary equipment or fixing method selected meets their requirements. This product is available in PDF format only. 4 pages
The effects of heat on scaffolding equipment can have a significant and permanent effect on its strength and performance. This guidance explains the potential issues and the action to be taken if equipment has been subjected to a fire or similar conditions. This guidance is available for pdf download only.
This guidance gives details of the stress corrosion cracking (SCC) that can occur in certain materials when subjected to tensile stress and specific corrosive environments. Although rare in our industry, it can lead to unexpected sudden failure of certain metals. Whilst chemical environments and alloys are highly specific, this guidance explains the process by which SCC can occur and advises that specialist advice may be needed where SCC is possible or has occurred in the past. This guidance is available for pdf download only.
2 pages
Scaffold tube storage racks are a common feature of every scaffolding contractor’s yard and many long-term live sites. Whilst tube racks are usually constructed as basic birdcage-like structures, they generally support many tonnes of equipment, so their design needs special consideration. This guidance note considers the design, use and maintenance of scaffold tube storage racks. 6 pages